Mechanical Properties Metric English Comments
Modulus of Elasticity 22.8 GPa
3300 ksi
Y; ASTM D3039
Park Electrochemical Nelco® N5000-30/32 BT Epoxy Package
The Nelco N5000-30 prepreg and N5000-32 laminate BT epoxy materials are designed specifically to meet or exceed new and emerging chippackaging requirements. The primary applications of these materia..
Modulus of Elasticity 22.8 GPa
3300 ksi
Y; ASTM D3039
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic..
Modulus of Elasticity 22.8 GPa
3300 ksi
Y; ASTM D3039
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform..