Polymer Property : Modulus of Elasticity = 210.3 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 210.3 GPa
30500 ksi
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13)
No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa..