Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.39 GPa | 202 ksi | Cross; ASTM D638 |
Arlon DiClad 880 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |