Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.714 - 15.13 GPa @Temperature -40.0 - 220 °C |
393.6 - 2194 ksi @Temperature -40.0 - 428 °F |
Average value: 7.37 GPa Grade Count:15 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |