Mechanical Properties Metric English Comments
Modulus of Elasticity 2.625 GPa
380.7 ksi
ISO 527
GEHR Plastics POM-ESD-FG Polyoxymethylene
Variant of POM (Copolymer) with an improved electrical conductivity. Surface resistivity =1011 O. Polyoxymethylene can be used in temperatures ranging from -58 °F to +230 °F. The high surface..