Material Notes:
Variant of POM (Copolymer) with an improved electrical conductivity. Surface resistivity =1011 O. Polyoxymethylene can be used in temperatures ranging from -58 °F to +230 °F. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and good resistance to wear because of the high strength and smooth surface. There is a very low risk of stress cracks.Information provided by GEHR Plastics, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
ISO 527
Tensile Strength, Yield 63.0 MPa
9140 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Modulus of Elasticity 2.625 GPa
380.7 ksi
ISO 527
Coefficient of Friction 0.20

@Temperature 60.0 °C
0.20

@Temperature 140 °F
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+12 ohm-cm
1.50e+12 ohm-cm
VDE 0303
Descriptive Properties Value Comments
Acid Resistance Yes
Aromatic Resistance Yes
Bondability No
CKW Resistance Limited
Hydrocarbonate Resistance Yes
Hydroxide Resistance Yes
Ketone Resistance Yes
Physiological indifference according No
Resistance to Hot Water Yes
UV Stabilization No