Mechanical Properties Metric English Comments
Modulus of Elasticity 3.70 - 12.9 GPa
537 - 1870 ksi
Average value: 8.84 GPa Grade Count:52
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..