Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Modulus of Elasticity | 178 GPa @Temperature 400 °C |
25800 ksi @Temperature 752 °F |
|
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |
|||
Modulus of Elasticity | 178 GPa | 25800 ksi | as rolled longitudinal |
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Modulus of Elasticity | 178 GPa @Temperature 700 °C |
25800 ksi @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |