Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.15 GPa | 167 ksi | ISO 527 |
GEHR Plastics PE-HD Polyethylene HDPE Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50.. |