Mechanical Properties Metric English Comments
Modulus of Elasticity 1.15 GPa
167 ksi
ISO 527
GEHR Plastics PE-HD Polyethylene HDPE
Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50..