Modulus of Elasticity |
140 - 160 GPa |
20300 - 23200 ksi |
Youngs Modulus |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-28EH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-28UH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-30EH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-30UH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-35 Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-35H Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-35M Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-35SH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-35UH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-38 Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-38SH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-40H Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-40M Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-40SH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-42M Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-42SH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-45M Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-50 Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-30EZ Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-33 Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-33H Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-33SH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-33UH Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-38H Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-38M Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-40 Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-42H Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-33M Neodymium Iron Boron Magnetic Material
|
Modulus of Elasticity |
150 - 160 GPa |
21800 - 23200 ksi |
|
Alliance N-48 Neodymium Iron Boron Magnetic Material
|