Polymer Property : Modulus of Elasticity = 16.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 16.8 GPa
2440 ksi
in <110> direction
Mateck Potassium Chloride (KCl)
Optical crystals
Modulus of Elasticity 16.8 GPa
2440 ksi
ISO 527-1/-2
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry)
Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF