Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 16.6 GPa | 2410 ksi | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |