Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 16.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 16.0 - 20.0 GPa
2320 - 2900 ksi
Injection; ISO 527
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Modulus of Elasticity 16.0 - 33.1 GPa
2320 - 4800 ksi
Average value: 21.6 GPa Grade Count:25
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 1105-8004 PEEK, with carbon fiber, low-warpage, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 1850-8282 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 20-0665 Polyphthalamide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 3/CF/30/EG Polyamide 6, with carbon fiber, extrusion grade
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 50-7844 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts; low thermal coefficient of expansion.Redu..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Modulus of Elasticity 16.0 GPa
2320 ksi
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Modulus of Elasticity 16.0 GPa
2320 ksi
ISO 527-1/-2
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Modulus of Elasticity 16.0 GPa
2320 ksi
DIN 53 457
Albis Plastics Tedur® P 9519 PPS, ~45% Glass Fiber (black only)
Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Handles, Fixing ElementsProcessing: Injec..
Modulus of Elasticity 16.0 GPa
2320 ksi
ISO 527-1/-2
BASF Ultramid® A3W2G10 BK 20560 50% Glass Filled PA66 (Dry)
Description: 50% glass fiber reinforced injection molding grade with optimized heat ageing performance for industrial articles having very high rigidity.Information provided by BASF
Modulus of Elasticity 16.0 GPa
2320 ksi
ISO 527-2
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..
Copyright © lookpolymers.com All Rights Reserved