Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 101 GPa | 14600 ksi | |
Wieland Auropal 1 Casting Alloy Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |
|||
Modulus of Elasticity | 101 GPa | 14600 ksi | |
Wieland Porta PressOver PFM Alloy High gold alloy for veneering with IMAGINE® h.e. press ceramicApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, acrylic veneeringDental |