Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wieland Auropal 1 Casting Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Silver Alloy
Manufacturer Wieland
Trade Name Auropal
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Auropal 1 Casting Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental
Physical Properties Metric English Comments
Density 14.3 g/cc
0.517 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 260
260
HV5/30; as cast
260
260
HV5/30; hardened
Tensile Strength, Yield 680 MPa

@Strain 0.200 %
98600 psi

@Strain 0.200 %
as cast
680 MPa

@Strain 0.200 %
98600 psi

@Strain 0.200 %
hardened
Elongation at Break 10 %
10 %
as cast
10 %
10 %
hardened
Modulus of Elasticity 101 GPa
14600 ksi
Component Elements Properties Metric English Comments
Copper, Cu 12 %
12 %
Gold, Au 63.4 %
63.4 %
Iridium, Ir <= 0.10 %
<= 0.10 %
Palladium, Pd 3.0 %
3.0 %
Platinum, Pt 0.50 %
0.50 %
Silver, Ag 19.5 %
19.5 %
Zinc, Zn 1.5 %
1.5 %
Processing Properties Metric English Comments
Processing Temperature 699 °C
1290 °F
Preheating Temp.
Melt Temperature 871 - 910 °C
1600 - 1670 °F
Casting Temperature 1060 °C
1940 °F
Descriptive Properties Value Comments
Color yellow