Mechanical Properties Metric English Comments
Modulus of Elasticity 125 GPa
18100 ksi
Osprey Metals CE7 Al-Si Controlled Expansion Alloy
Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Modulus of Elasticity 125 GPa
18100 ksi
SGL Carbon Group SIGRAFIL C® in 250°F Epoxy
60% fiber volumeInformation provided by SGL Carbon Group
Modulus of Elasticity 125 GPa
18100 ksi
Typical
TIMET 8-1-1 Titanium Alloy (Ti-8Al-1Mo-1V); Annealed Sheet
Industry Specifications: USA Aerospace: AMS 4915,4916. France: T-A8DV. Features: Designed for creep resistance up to 450°C, used primarily in engine applications such as forged compressor blades..
Modulus of Elasticity 125 GPa
18100 ksi
Typical
TIMET TIMETAL® 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) Titanium Alloy
High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: Germany Aerospace: 3.7154. France: T-A6ZD. UK Aerospace Specifications BS TA. 43, 44.Features: TIMETAL 685 possesses ..
Modulus of Elasticity 125 GPa
18100 ksi
UD
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..
Modulus of Elasticity 125 GPa
18100 ksi
ASTM E494
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite
High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co..