SGL Carbon Group SIGRAFIL C® in 250°F Epoxy

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite , Filled/Reinforced Thermoset
Manufacturer SGL Carbon Group
Trade Name SIGRAFIL C®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group SIGRAFIL C® in 250°F Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60% fiber volumeInformation provided by SGL Carbon Group
Mechanical Properties Metric English Comments
Tensile Strength at Break 1900 MPa
276000 psi
Modulus of Elasticity 125 GPa
18100 ksi
Flexural Strength 1600 MPa
232000 psi
Flexural Modulus 120 GPa
17400 ksi
Compressive Strength 1300 MPa
189000 psi
Compressive Modulus 120 GPa
17400 ksi
Shear Strength 82.7 - 96.5 MPa
12000 - 14000 psi