Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Pacific Sintered Materials F-240-S Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-25All information provided by Pacific Sintered Metals. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915â„¢ Annealed Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Modulus of Elasticity | 124 GPa @Temperature 871 °C |
18000 ksi @Temperature 1600 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915â„¢ Annealed Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915™ AT Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Schott N-LAF21 Glass Information Provided by SCHOTT North America, Inc. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TD01 1/4 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TD02 1/2 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TD04 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TM02 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TM06 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TS01 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TS03 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TS04 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Modulus of Elasticity | 124 GPa | 18000 ksi | |
Ametek AM 388™ Alloy (UNS C72650) TX00 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |