Modulus of Elasticity 0.786 GPa
114 ksi
ASTM D638
Huntsman Rexell® H2109 Injection Molding LLDPE  (discontinued **)
Linear-low high density injection molding.Features: High flow, good ESCR.Applications: General purpose molding, housewares.Information provided by Huntsman Corporation