Polymer Property : Modulus of Elasticity = 114 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 107 - 114 GPa
15500 - 16500 ksi
Typical
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32)
High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f..