Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0689 - 1.90 GPa
10.0 - 275 ksi
Average value: 0.579 GPa Grade Count:25
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..