Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.515 GPa | 219.7 ksi | ASTM D638 |
Total PPH 3281 Polypropylene, Extrusion Grade Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, result.. |
|||
Modulus of Elasticity | 1.515 GPa | 219.7 ksi | ASTM D638 |
Total PPH 3480Z Polypropylene, Extrusion Grade Homopolymer Profile Extrusion GradeProcess Stability --FINA 3480Z is formulated specifically to give excellent process stability in high profile extrusion.High Purity - Low catalyst residues in FINA.. |
|||
Modulus of Elasticity | 1.515 GPa | 219.7 ksi | ASTM D638 |
Total PPH 3462 Polypropylene, Extrusion Grade Homopolymer extrusion grade for slit film and fibrillated tapesProcess Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.FDA - FINA 3462 complies with.. |