Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3281 Polypropylene, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low melt flow homopolymer for sheet extrusion, strapping, and in-line thermoforming applicationsMelt Strength – The high melt strength of FINA 3281 allows uniform drawdown during processing, resulting in maximum line speeds and a good balance of physical properties.Process Stability – Excellent polymer stability of FINA 3281 produces consistent product properties during extrusion, even with the use of regrind.FDA – FINA 3281 complies with all applicable FDA regulations and may be used under these provisions for food contact applications.Recommended Applications -- FINA 3281 is recommended for sheet and strapping applications where high melt strength and high extrusion speeds are required.Processing – FINA 3281 resin processes on conventional extrusion equipment with typical melt temperatures of 390-450°F (200-232°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 1.1 g/10 min
1.1 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D288A
Hardness, Shore D 81
81
ASTM D1706
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Modulus of Elasticity 1.515 GPa
219.7 ksi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256A
Izod Impact, Unnotched 15.9 J/cm
29.8 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 165 °C
329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 200 - 232 °C
392 - 450 °F
Extrusion