Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 1.015 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.015 GPa
147.2 ksi
ASTM D638
Flint Hills PP 23R2A Random Copolymer Polypropylene
Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: High contact clarity, non-blushing, toughness, impact, chemical..
Copyright © lookpolymers.com All Rights Reserved