Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.490 - 0.780 GPa | 71.1 - 113 ksi | ASTM D638 |
Zeus EFEP Tubing |
|||
Modulus of Elasticity | 0.490 - 0.780 GPa | 71.1 - 113 ksi | ASTM D638 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |