Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.738 GPa | 107 ksi | Molded Sample 2% Secant Modulus |
Dow DOWLEX™ IP-10262 High Density Polyethylene DOWLEX® IP-10262 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution for use in reusable case applications including, poultry, fast food, a.. |