Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.250 GPa | 36.3 ksi | TD; ISO R527-1 |
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi.. |
|||
Modulus of Elasticity | 0.250 GPa | 36.3 ksi | MD; ISO 527 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Modulus of Elasticity | 0.250 GPa | 36.3 ksi | ISO 527-2 |
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Pe.. |