Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 0.116 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.000800 GPa
0.116 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8550 (GFLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued
FormulationVTR-8550
Modulus of Elasticity 0.000800 GPa
0.116 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8505/8500 Formulation  (discontinued **)
FormulationViton® 8505
Modulus of Elasticity 0.000800 GPa
0.116 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8655 (GBL-S) , VTR 8650 8655/8650 Blend  (discontinued **)
FormulationVTR 8655
Copyright © lookpolymers.com All Rights Reserved