Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0190 GPa
2.76 ksi
ASTM D638
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e..
Modulus of Elasticity 0.0190 GPa
2.76 ksi
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..