Polymer Property : Modulus of Elasticity = 0.00550 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.00550 GPa
0.798 ksi
Silicone Property; Arlon-SAQ-TMS-008
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..
Modulus of Elasticity 0.00550 GPa
0.798 ksi
Silicone Property; Arlon-SAQ-TMS-008
Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..