Polymer Property : Modulus of Elasticity = 0.0006998 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0006998 GPa
0.1015 ksi
Dow Corning JCR 6126 W/C
Two-part, translucent, thixotropic, medium modulus LED encapsulant with a very long working time.Information provided by Dow Corning