Dow Corning JCR 6126 W/C

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning JCR 6126 W/C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, translucent, thixotropic, medium modulus LED encapsulant with a very long working time.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 26
26
Tensile Strength, Ultimate 1.800 MPa
261.1 psi
Modulus of Elasticity 0.0006998 GPa
0.1015 ksi
Optical Properties Metric English Comments
Refractive Index 1.396
1.396
1.404
1.404
1.395

@Wavelength 1554 nm
1.395

@Wavelength 1554 nm
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month