Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 825 MPa
120000 psi
ISO 899
BASF Ultraform N 2640 Z6 UNC POM
Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength.