Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 825 MPa | 120000 psi | ISO 899 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |