Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 5100 MPa | 740000 psi | ISO 899-1 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Tensile Creep Modulus, 1 hour | 5100 MPa | 740000 psi | ISO 899-1 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Tensile Creep Modulus, 1 hour | 5100 MPa | 740000 psi | ISO 899-1 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
Tensile Creep Modulus, 1 hour | 5100 MPa | 740000 psi | ISO 899-1 |
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber PA 6, Injection molding grade, 30% glass fibers, weather stabilized |