Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1800 - 2200 MPa
261000 - 319000 psi
Average value: 2080 MPa Grade Count:5
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Tensile Creep Modulus, 1 hour 1600 - 2200 MPa
232000 - 319000 psi
Average value: 1930 MPa Grade Count:3
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..