Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 1800 - 2200 MPa
261000 - 319000 psi
Average value: 2080 MPa Grade Count:5
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Tensile Creep Modulus, 1 hour 1800 - 2500 MPa
261000 - 363000 psi
Average value: 2280 MPa Grade Count:11
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Tensile Creep Modulus, 1 hour 1800 - 2700 MPa
261000 - 392000 psi
Average value: 2460 MPa Grade Count:9
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Tensile Creep Modulus, 1 hour 1800 MPa
261000 psi
Arkema Group Oroglas® HFI-7 Acrylic  (discontinued **)
OROGLAS HFI-7 is a medium impact grade that in addition to the improvement in impact resistance provides superior flow which contribute to reduce the cycle time and improve demolding.Key features :..
Tensile Creep Modulus, 1 hour 1800 MPa
261000 psi
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep..
Tensile Creep Modulus, 1 hour 1800 MPa
261000 psi
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe)
Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF.
Tensile Creep Modulus, 1 hour 1800 MPa
261000 psi
ISO 899
BASF Ultraform H 2320 006 Q600 POM
Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470.
Tensile Creep Modulus, 1 hour 1800 MPa
261000 psi
ISO 899
BASF Ultraform N 2320 U03 UNC Q600 POM
Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade.
Tensile Creep Modulus, 1 hour 1800 MPa
261000 psi
Arkema Group Oroglas® SG 7 Acrylic, Gamma Radiation Resistant  (discontinued **)
OROGLAS SG 7 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse ..