Polymer Property : Tensile Creep Modulus, 1 hour = 305000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2100 - 5900 MPa
305000 - 856000 psi
Average value: 2400 MPa Grade Count:25
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Tensile Creep Modulus, 1 hour 2100 - 8500 MPa
305000 - 1.23e+6 psi
Average value: 4550 MPa Grade Count:6
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Tensile Creep Modulus, 1 hour 2100 MPa
305000 psi
Covestro Makrolon® 2205 Polycarbonate, Injection Grade
Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc..
Tensile Creep Modulus, 1 hour 2100 MPa
305000 psi
Covestro Makrolon® 2207 Polycarbonate, Injection Grade
Exceptionally good flow injection molding grade with easy mold release and UV stabilizer, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015..
Tensile Creep Modulus, 1 hour 2100 MPa
305000 psi
ISO 899-1
Covestro Makrolon® 2258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Tensile Creep Modulus, 1 hour 2100 MPa
305000 psi
ISO 899
BASF Ultraform W 2320 003 UNC Q600 POM
Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains ..
Tensile Creep Modulus, 1 hour 2100 MPa
305000 psi
ISO 899-1
Covestro Makrolon® LED2245 Polycarbonate
ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature..