Polymer Property : Tensile Creep Modulus, 1 hour = 1.23e+6 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 2100 - 8500 MPa
305000 - 1.23e+6 psi
Average value: 4550 MPa Grade Count:6
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..