Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 80.0 kJ/m²
38.1 ft-lb/in²
Notched, -30°C; ISO 8256
Total Finathene® 6002 HDPE, blow molding, pipe  (discontinued **)
FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b..
Tensile Impact Strength 80.0 kJ/m²
38.1 ft-lb/in²
At 23°C; ISO 8256/A1
Borealis Borstar® MB7541 High Density Polyethylene for Injection Molding
Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan..
Tensile Impact Strength 80.0 kJ/m²
38.1 ft-lb/in²
Notched, -30°C; ISO 8256
Total 5502 HDPE, blow molding, pipe
Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified
Tensile Impact Strength 80.0 kJ/m²
38.1 ft-lb/in²
At 23°C; ISO 8256/A1
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding
Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan..
Tensile Impact Strength 80.0 - 480 kJ/m²
38.1 - 228 ft-lb/in²
Average value: 243 kJ/m² Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Tensile Impact Strength 80.0 kJ/m²
38.1 ft-lb/in²
ISO 8256/A1
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications
Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESC..