Tensile Impact Strength 146 - 815 kJ/m²
69.5 - 388 ft-lb/in²
Average value: 596 kJ/m² Grade Count:16
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Tensile Impact Strength 146 kJ/m²
69.5 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-724 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty compounding applications. Outstanding heat sealability along with excellent strength properties ..