Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 146 - 815 kJ/m² | 69.5 - 388 ft-lb/in² | Average value: 596 kJ/m² Grade Count:16 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |