Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 610 kJ/m² | 290 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |