Polymer Property : Tensile Impact Strength = 290 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 610 kJ/m²
290 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-728 High EVA Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams..