Tensile Impact Strength 600 kJ/m²
286 ft-lb/in²
23°C; ASTM D-1822
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr..