Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 600 kJ/m² | 286 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |