Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Impact Strength = 46.2 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 46.2 kJ/m²
22.0 ft-lb/in²
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black
Information provided by ITW Devcon
Tensile Impact Strength 46.2 kJ/m²
22.0 ft-lb/in²
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive, Straw, White, Black
Information provided by ITW Devcon
Copyright © lookpolymers.com All Rights Reserved