Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 46.2 kJ/m² | 22.0 ft-lb/in² | |
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black Information provided by ITW Devcon |
|||
Tensile Impact Strength | 46.2 kJ/m² | 22.0 ft-lb/in² | |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive, Straw, White, Black Information provided by ITW Devcon |