Mechanical Properties Metric English Comments
Tensile Impact Strength 94.5 kJ/m²
45.0 ft-lb/in²
Type S; ASTM D1822
Chase Plastics CP Pryme® AC125 Acetal Copolymer, 25% Glass Fiber Reinforced
Features: Glass fiber reinforcedAlkali resistantGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantResilientHigh rigid..
Tensile Impact Strength 94.5 kJ/m²
45.0 ft-lb/in²
ASTM D-1822
Axiall HHW-191 Rigid PVC, Extrusion
Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic..
Tensile Impact Strength 94.5 kJ/m²
45.0 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ BA7794 Sheet Extrusion and Blow Molding Resin  (discontinued **)
BA7794 is a 25% talc-filled, high molecular weight, high density polyethylene. This color match-able material has been specifically developed as a cost effective resin for applications which requir..